Synonymous:Cis-1,4-polyisoprene rubber, polyisoprene rubber, isoprene rubber.
Product Introduction:
Luhua Isoprene Rubber (LHIR) is a polyisoprene with a high cis-1,4 content and high molecular weight. LHIR is milky white, homogeneous and low in impurities, shows good flowability and mixability.
Packaging:25.0kg multiwall paper bags
Storage:Store at room temperature, avoid heat and light.
Product Application:
LHIR is suitable for all applications of natural rubber, such as tires, tapes, hoses, shoes and other rubber products, and offers many advantages which are not found in natural rubbers, including high purity, low gel content, homogeneous, transparency and luster among others, make it possible to produce products which require high degree of purity and molecular regularity. For example, it can be used to produce packaging and sealing of foods and pharmaceuticals, medical plugs and gaskets, baby bottle nipples, health care materials, adhesives and very light colored or transparent rubber products.
Technical Parameter :
Properties | LHIR60 | LHIR70 | LHIR80 | LHIR90 |
Appearance | Milky white semi-transparent solid | |||
Mooney Viscosity, ML | 55-64 | 65-74 | 75-84 | 85-95 |
Deviation of Mooney viscosity of each batch ≤ | ±4 | ±4 | ±4 | ±4 |
Tensile strength,MPa23℃≥ | 21.5 | 21.5 | 21.5 | 21.5 |
Tear strength,KN/m | 30 | 30 | 30 | 30 |
Elongation at break,%,≥ | 700 | 700 | 700 | 700 |
Volatiles %,≤ | 0.7 | 0.7 | 0.7 | 0.7 |
Ash,%,≤ | 0.5 | 0.5 | 0.5 | 0.5 |
Fe,%,≤ | 0.003 | 0.003 | 0.003 | 0.003 |
Cu%,≤ | 0.0001 | 0.0001 | 0.0001 | 0.0001 |
anti-aging agent %,≤ | 1.0 | 1.0 | 1.0 | 1.0 |